Three-Dimensional Printing Of Transparent Fused Silica Glass

Glass is one of the most important high-performance materials used for scientific research, in industry and in society, mainly owing to its unmatched optical transparency, outstanding mechanical, chemical and thermal resistance as well as its thermal and electrical insulating properties. However, glasses and especially high-purity glasses such as fused silica glass are notoriously difficult to shape, requiring high-temperature melting and casting processes for macroscopic objects or hazardous chemicals for microscopic features. These drawbacks have made glasses inaccessible to modern manufacturing technologies such as 3D printing. However, using a casting nanocomposite, this article reports how a transparent fused silica glass component using sterolithography 3D printers at resolutions of a few tens of micrometers was created. The process uses a photocurable silica nanocomposite that is 3D printed and converted to high-quality fused silica glass via heat treatment.

Author
F Kotz Et Al
Origin
Imt, Germany
Journal Title
Nature 544 April 2017 337-341
Sector
Special Glass
Class
S 4356

Request article (free for British Glass members)

Three-Dimensional Printing Of Transparent Fused Silica Glass
Nature 544 April 2017 337-341
S 4356
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.