Thorium Free Optical Glass Of High Refractive Index

Covers range (wt%): 20-40 B2O3, 40-60 La2O3, 0-1 ZrO2, 0-31 Ta2O5 and specifically two compositions, in the same order, 30, 53, 5, 12 and 33, 52, 10, 5. Some 30 composiions are listed with RI 1.747-1.873.