Thin Glass Film Between Ultrafine Conductor Particles In Thick-Film Resistors

Thick-film resistors are electrical composites comtaining ultrafine particles of ruthenate conductor (Pb2Ru2O7 in the present materials) distributed in a highly modified silicate glass. This article shows that conductor particles remain flocced in the absence of any applied or capiliary pressures, but are separated at equilibrium by a nanometer-thick film of glass. Microstructures show evidence for liquid-phase sintering, i.e., contact flattening of particles, under van der Waals attraction alone.

Author
Y-Ming Chiang Et Al
Origin
Massachusetts Inst Of Technology, Usa
Journal Title
J Am Ceram Soc 77 5 1994 1143-1152
Sector
Special Glass
Class
S 810

Request article (free for British Glass members)

Thin Glass Film Between Ultrafine Conductor Particles In Thick-Film Resistors
J Am Ceram Soc 77 5 1994 1143-1152
S 810
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.