Thickness Of Thin Films On Glass - A Round Robin Test

The film thicknesses of five different layer systems on glass substrates were analysed and determined in a multi-method approach by eight different university and industrial laboratories. The total coating thicknesses varied between a few nm up to some 100nm. The measurements give information about the chemical composition and cover a wide spectrum of typical coating application on glasses. The results of the different laboratories and methods are compared and the challenges and limits of the various analytical techniques are discussed.

Author
V Rupertus Et Al
Origin
Schott, Germany
Journal Title
Glass Sci Technol 78 5 2005 212-217
Sector
Special Glass
Class
S 3028

Request article (free for British Glass members)

Thickness Of Thin Films On Glass - A Round Robin Test
Glass Sci Technol 78 5 2005 212-217
S 3028
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.