Thickness Measurement In The Automated Testing Laboratory

In this article, the author describes a glass container thickness measurement gauge that provides the means to capture precision thickness data in a highly effective and economical manner, overcoming many of the issues associated with hand or on-line measurements.

Author
D Dineff
Origin
Agr International, Usa
Journal Title
Glass Worldwide Jan-Feb/2013 70-72
Sector
Container glass
Class
C 4811