The Thermos Flask

The basic Thermos brand flask consists of two glass containers with a vacuum between them, placed inside a metal or plastic casing. The glass used is of the borosilicate variety. This paper briefly describes the process involved in making these flasks.

Author
Un-named
Origin
Unknown
Journal Title
Glass 75 11 1998 375