Thermodynamics Of Redox Equilibria And Diffusion Of Polyvalent Ions In A Phosphate Glass Melt

A phosphate glass melt with the basic composition of NaPO3.2Sr(PO3)2 doped with various oxides of polyvalent elements was studied with the aid of square-wave voltammetry. The standard potentials depended linearly on temperature. The diffusion coefficients were determined from current densities obtained and fulfilled the Arrhenius' law. Both thermodynamics of the redox equilibria and diffusion coefficients are compared with those measured in soda-lime-silica glasses.

Author
A Matthai Et Al
Origin
Otto-Schott Inst, Germany
Journal Title
Glastech Ber Glass Sci Technol 71 2 1998 29-34
Sector
Special Glass
Class
S 1330

Request article (free for British Glass members)

Thermodynamics Of Redox Equilibria And Diffusion Of Polyvalent Ions In A Phosphate Glass Melt
Glastech Ber Glass Sci Technol 71 2 1998 29-34
S 1330
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.