Thermodynamic Properties Of Manganese Oxides

Transposed temperature drop calorimetry and high-temperature drop solution calorimetry in molten 2Pb0.B203 at 977K were used to study the energetics of some manganese oxides, namely pyrolusite (Mn02), bixbyite (Mn203), hausmannite (Mn304), and manganosite (Mn0). Using new values of enthalpies and reliable standard entropies, the phase-stability diagram of the manganese-oxygen system was constructed.

Author
S Fritsch & A Navrotsky
Origin
Princeton Materials Inst, New Jersey, Usa
Journal Title
J Am Ceram Soc 79 7 1996 1761-1768
Sector
General
Class
G 1503

Request article (free for British Glass members)

Thermodynamic Properties Of Manganese Oxides
J Am Ceram Soc 79 7 1996 1761-1768
G 1503
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.