Thermodynamic Aspects Of Pressure-Induced Crystallization: Kauzmann Pressure

General equations for the dependence of the thermodynamic driving force and the specific interfacial energy melt-crystal of critical clusters on temperature and pressure are derived. Analytical estimates of these and related thermodynamic quantities are advanced directly applicable in the analysis of experimental data of crystal nucleation. Similar to the well-known notation of a Kauzmann temperature, the concept of a Kauzmann pressure is introduced. It is shown that the thermodynamic driving force of crystal nucleation has a maxima not only at the Kauzmann temperature but also at the Kauzmann pressure. Estimates of the magnitude of the thermodynamic driving force of cyrstallization at these states are given and some consequences are discussed.

Author
J W P Schmelzer Et Al
Origin
Inst Physics, University Rostock, Germany
Journal Title
Int J Appl Glass Sci 7 4 2016 474-485
Sector
Special Glass
Class
S 4307

Request article (free for British Glass members)

Thermodynamic Aspects Of Pressure-Induced Crystallization: Kauzmann Pressure
Int J Appl Glass Sci 7 4 2016 474-485
S 4307
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.