Thermodynamic Aspects Of Melting And Glass Formation

Glasses are mostly produced by cooling from the melt. In order to understand the mechanism of melting & glass formation, the enthalpy function & the specific heat capacities of one-component systems have been analysed. In many cases, the specific heat capacity due to atomic vibrations is increased near the melting transition by a contribution due to electronic transitions from low to high energy levels. These electronic transitions, which increase with the temperature, are accompanied by a change of the corresponding wave-functions & of the local charge distributions. The charge distribution changes according to the random time series of the different occupied electronic states & drives the core ions into new positions.

Author
Hj Hoffmann
Origin
Inst Materials Science & Technology, Berlin, Germany
Journal Title
Physics & Chemistry Of Glasses 48 1 Feb 2007 23
Sector
Special Glass
Class
S 3281

Request article (free for British Glass members)

Thermodynamic Aspects Of Melting And Glass Formation
Physics & Chemistry Of Glasses 48 1 Feb 2007 23
S 3281
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.