Thermodynamic Analysis Of The Tin Penetration Profile In High-Iron Float Glass

The chemical interactions that occur between tin and molten glass during the float forming process were investigated using experimental techniques & theoretical modeling calculations. The characteristic bump in the tin penetration profile commonly observed in the bottom side of green commercial float glasses was reproduced in laboratory float experiements. Thermodynamic modeling calculations revealed the existence of a steep gradient in the oxygen activity between the highly-reduced tin bath & the relatively oxidized float glasses. The tin penetration profiles of two high-iron glasses floated in the laboratory were deconvoluted into Sn2+ & Sn4+ components, according to the proposed oxygen activity gradient. Accdording to the calculations, the bump in the tin profile is associated with the accumulation of Sn4+ in a localized region.

Author
T E Paulson Et Al
Origin
Pennsylvania State University, Usa
Journal Title
Proc Xviii Icg, San Francisco, Usa, July 1998 165-170
Sector
Special Glass
Class
S 1856

Request article (free for British Glass members)

Thermodynamic Analysis Of The Tin Penetration Profile In High-Iron Float Glass
Proc Xviii Icg, San Francisco, Usa, July 1998 165-170
S 1856
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 13 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.