Thermal Performance Of Aluminum And Glass Beer Bottles

Aluminium beer bottles recently have been introduced as an alternative to traditional glass bottles or aluminium cans. Advertisements claim that the new aluminium bottles keep beer "colder longer" than glass bottles. Because the thermal conductivity of aluminium is over 150 times that of typical soda/lime glass and because the bottle wall is thinner, this claim appears counterintuitive. In this investigation, the thermal performance of commercially available aluminium and glass beer bottles was examined using experimental, analytical and computational methods. It was found that when exposed to ambient air, glass and aluminum bottles perform in a nearly identical manner with respect to keeping their contents cold. Each bottle showed an approximately 15 degrees C temperature rise over a period of about 2 hours 40 minutes. Heat transfer is controlled by natural convection and thermal radiation at the outer bottle surface; hence, the difference in thermal conductivity between the bottles has no significant impact on the temperature transient. Computational simulations also predict that when an aluminium bottle is immersed in an ice water bath, the liquid cools more quickly than in glass due to the lower thermal resistance of the aluminium versus the glass; when held in the hand, the glass bottle allows the liquid to warm more slowly than the aluminium bottle.

Author
R T Bailey & W L Elban
Origin
Unknown
Journal Title
Heat Tranfer Eng 29 7 July 2008 643-650
Sector
Container glass
Class
C 4504

Request article (free for British Glass members)

Thermal Performance Of Aluminum And Glass Beer Bottles
Heat Tranfer Eng 29 7 July 2008 643-650
C 4504
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.