Thermal Non-Linearity Of Sodium Disilicate Glasses Doped With Mn

The photothermal deflection method in linear configuration has been applied to measurement of the non-linearity of sodium disilicate glasses doped with manganese, with different heat treatments.

Author
M Bertolotti Et Al
Origin
"La Sapienza" University, Rome, University Of Parma
Journal Title
Rivista Della Staz Sper Vetro 1989 1 165-168
Sector
Special Glass
Class
S 283