Thermal Homogeneity Index - The Real Truth

At present, temperature distribution across the channel cross section is regarded as an adequate substitute, being both easy & cheap to measure. The accepted method of measuring the temperature distribution uses 3 triplex thermocouples, which are normally installed vertically through the roof, & are designed to provide temperature readings at 3 different levels. To allow easy comparison of various sets of readings, the 9 temperature values of a single data set are treated mathematically to give a value, which is normally quoted as a percentage. If all of these are the same the formula will give a value of 100, which is referred to as the Thermal Homogeneity Index (THI). However, there is little information concerning the practical aspects of this type of measurement & in particular, the various inaccuracies that are inherent in the measurement.

Author
J Grossler
Origin
Nikolaus Sorg Gmbh, Germany
Journal Title
Glass Sept/05 22-24
Sector
Container glass
Class
C 2841

Request article (free for British Glass members)

Thermal Homogeneity Index - The Real Truth
Glass Sept/05 22-24
C 2841
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
15 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.