Thermal Expansion Kinetics - Method To Measure Permeability Of Cementitious Materials: Iii, Effect Of Viscoelasticity

When a porous material that is saturated with liquid is heated, the liquid expands much more than the solid phase. If the permeability is low, then the liquid may not be able to escape as it expands, so that it expands within the pores and causes dilation of the body. In that case, by analysing the kinetics of dilation during a change in temperature, it is possible to extract the permeability. The behaviour of an elastic porous solid was analysed previously. In this paper the case of a viscoelastic material is considered; for cementitious materials the effect of a relaxation is shown to be significant, but the elastic analysis will usually provide sufficient accuracy. If significant viscoelastic relaxation occurs, it is revealed by comparing the data from samples of different sizes.

Author
G W Scherer
Origin
Princeton University, Usa
Journal Title
Jacs 87 8 2004 1509-1516
Sector
General
Class
G 2935

Request article (free for British Glass members)

Thermal Expansion Kinetics - Method To Measure Permeability Of Cementitious Materials: Iii, Effect Of Viscoelasticity
Jacs 87 8 2004 1509-1516
G 2935
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 12 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.