[Thermal Endurance] Resistance Of Glass To Changes In Temperature

In this article the author examines the thermal endurance of glass articles to sudden fluctuations in temperature and discusses reduction in the coefficient of heat expansion of articles, strengthening of glass articles by ion exchange, and strengthening of glass articles by coating with a thin glass layer with a different coefficient of heat expansion.