Thermal Analysis Of Reactions In Soda-Lime Silicate Glass Batches Containing Melting Accelerants: 1, One- And Two-Component System

Thermal analysis of reactions in soda-lime silicate glass batches, containing melting accelerants is undertaken.

Author
K S Hong, R F Speyer
Origin
Alfred University, Usa
Journal Title
J Am Ceram Soc 76 3 1993 598-604
Sector
Special Glass
Class
S 714

Request article (free for British Glass members)

Thermal Analysis Of Reactions In Soda-Lime Silicate Glass Batches Containing Melting Accelerants: 1, One- And Two-Component System
J Am Ceram Soc 76 3 1993 598-604
S 714