The melting reactions in a sodium-potassium-lead silicate glass batch were studied simultaneously by D T A, TG, and DTG in conjunction with x-ray diffraction analysis to identify the phases which formed during heat treatment. The batch using ground (-325 mesh) tribasic lead silicate underwent low temperature reactions, ultimately forming at about 850 C a liquid which contained all of the alkali and lead oxide and some of the silica. The use of granular (-10+80mesh) tribasic lead silicate resulted in the formation of two liquid phases, of substantially different densities,which assimilated the remaining silica, but did not form a single homogeneous melt.

Author
W R Ott Et Al
Origin
Unknown
Journal Title
Glass Technol 13 1972 154-60
Sector
Primary Papers
Class
PP 1292

Request article (free for British Glass members)

Thermal Analysis Of Lead Glass Batch
Glass Technol 13 1972 154-60
PP 1292
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
10 + 9 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.