Thermal Analysis Of Glass Covered Amorphous Metal Wire And Amorphous Ribbon

Glass covered amorphous metal wires (GCAW) of compositions Co66Fe4Ni1Si15B14, Co68.28Fe4.32Si12.5B15, and Fe9Si19B12, and Fe9Si19B2 amorphous metal ribbon were thermally characterised using differential scanning calorimetry, modulated differential scanning calorimetry, and thermogravimetric analysis.