Thermal Analysis Of Ge-S Glasses

A study has been made of the thermal behaviour of Ge-S glasses using differential thermal analysis and thermogravimetric analysis. Crystalline products formed during thermal analysis were identified by x-ray diffraction.

Author
Y Kawamoto & S Tsuchihashi
Origin
Unknown
Journal Title
Journal Of The American Ceramic Society 54 10 1971 526-527
Sector
Primary Papers
Class
PP 1305

Request article (free for British Glass members)

Thermal Analysis Of Ge-S Glasses
Journal Of The American Ceramic Society 54 10 1971 526-527
PP 1305