Theoretical Model Of Phosphorus Incorporation In Silica In Modified Chemical Vapor Deposition

Based on experiment, a theoretical model is developed of phosphorus incorporation in modified chemical vapour deposition. The results apply to viscous sintering of glasses produced by flame hydrolosis and sol-gel processes.

Author
D J Digiovanni, T F Morse, J W Cipolla
Origin
Brown University, Northeastern University
Journal Title
J Am Ceram Soc 1988 71 11 914-923
Sector
Glass Fibre
Class
GF 29