Theoretical Analysis Of The Dissolution Of Multi-Component Gas Bubbles

Numerical methods have been developed to compute accurately the behaviour of multi-component gas bubbles which either grow or dissolve on conditions of spherical symmetry.

Author
M Cable, J R Frade
Origin
University Of Sheffield
Journal Title
Glastech Ber 1987 60 11 355-362
Sector
General
Class
G 57

Request article (free for British Glass members)

Theoretical Analysis Of The Dissolution Of Multi-Component Gas Bubbles
Glastech Ber 1987 60 11 355-362
G 57