Testures In Glass Ceramics Of The System Li2O-Al2O3-Sio2

A bulk glass and a thin sol-gel film near the molar composition Li2O.Al2O3.SiO2. were crystallized by appropriate heat treatments. Whereas the interior of the glass displayed randomly oriented spodumene crystals, the rim showed an alignment of the crystals normal to the surface. With X-ray pole figure measurements a (111) fibre texture could be confirmed. Atomic force microscope images also proved an orientation in the crystallized film and the pole figures confirmed a similar fibre texture as in the case of the crystalline surface layer on the bulk material.

Author
W Michael Et Al
Origin
Inst Nichmetallische, Clausthal, Germany
Journal Title
Glastech Ber Glass Sci & Technol 73 C1 2000 98-103
Sector
Glass Ceramics
Class
GC 795

Request article (free for British Glass members)

Testures In Glass Ceramics Of The System Li2O-Al2O3-Sio2
Glastech Ber Glass Sci & Technol 73 C1 2000 98-103
GC 795
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 12 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.