Tests Establish Laminated Glass Strengths

Three years of scientific research at Texas Tech University's Glass Research & Testing Laboratory (GRTL) In Lubbock, Texas, has provided in-depth data on the strength and behaviour of laminated glass units under loads representing wind pressure. This data forms the basis for establishing relationships between the strength of laminated glass units and the strength of monolithic glass with the same nominal geometry and glass type.