A Testing Station For Glass Container Pressure Strength

AGR International's SPT2 automated pressure and volume measurement system offers technology and efficiency for glass bottle testing at the production line. The SPT2 can automatically test and collect pressure and volume data on bottles selected for sampling, without operator intervention, on a 24/7 basis at a rate of up to 270/bph.