Test Results Of In-Flight Glass Melting Using One-Ton/Day Large Scale Experimental Melter

This paper explains how the granulated batch can be vitrified in the oxy-gas flame. No seeds over 1mm were found in the melted glass. The analysed Na2O% is 15.4% while the analysed batch of Na2O was 15.6%. One pair of screw type stirrers gave good glass homogeneity. The melted glass had low Fe3/Fe2 ratio. The Rapidox measurement of the melted glass showed low oxygen activity. Current specific heat with this experimental furnace is around 4.45GJ/ton-glass.

Author
M Iwamoto Et Al
Origin
Toyo Glass, Japan
Journal Title
Ceramic Transactions Vol 231 2012 51-58 (Proc 9Th Int Conf On Advances In Fusion (Afpg9), Australia
Sector
General
Class
G 4644c

Request article (free for British Glass members)

Test Results Of In-Flight Glass Melting Using One-Ton/Day Large Scale Experimental Melter
Ceramic Transactions Vol 231 2012 51-58 (Proc 9Th Int Conf On Advances In Fusion (Afpg9), Australia
G 4644c
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.