On Terminal Crack Velocities In Glasses

A review of the literature shows that terminal crack velocity should be correlated with the longitudinal elastic wave velocity, and the structure and density of glasses. Theoretical predictions of Vct by the Mott-Roberts-Wells model match experimental measurements for some key glasses, including fused silica and low density borosilicates. It is suggested that the slower Vct results obtained for many other glasses are due to structural variations that cause crack front perturbations. The conclusions of this paper are most likely applicable to ceramics as well.

Author
G D Quinn
Origin
Nist, Maryland, Usa
Journal Title
Int J Appl Glass Sci January 2019 7-16
Sector
Special Glass
Class
S 4496

Request article (free for British Glass members)

On Terminal Crack Velocities In Glasses
Int J Appl Glass Sci January 2019 7-16
S 4496
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 13 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.