Tensile Strengths Of Se, As2S3, As2Se3, And Ge30As15Se55 Glass Fibers

The strengths of as-drawn, abraded, and pristine selenium, arsenic selenide, arsenic sulphide and germanium arsenic selenide fibres are reported.