Temperature-Modulated Differential Scanning Calorimetry Analysis Of High-Temperture Silicate Glasses

Recent advances in high-temperature experiments on commercial instruments could enable temperature-modulated differential scanning calorimetry as a method to investigate industrially relevant silicate glasses.

Author
T K Bechgaard Et Al
Origin
Aalborg University, Denmark
Journal Title
Am Ceram Soc Bull 97 4 2018 31-33