Temperature Effects On Laminated Glass At High Rate

The load bearing capacity of a laminated glass pane changes with temperature. In blast protection, laminated glass panes with a Polyvinyl Butyral (PVB) interlayer are usually employed. The post-crack response of the laminated pane is determined by the interlayer material response and its bond to the glass plies. An experimental study has been performed to determine the effects of temperature on the post cracked response of laminated glass at a test rate of 1 m/s for PVB thicknesses of 0.76 mm, 1.52 mm and 2.28 mm. Tensile tests were carried out on single cracked and randomly cracked samples in a temperature range of 0 °C–60 °C. Photoelasticity observation and high speed video recording were used to capture the delamination in the single cracked tests. Competing mechanisms of PVB compliance and the adhesion between the glass and PVB, were revealed. The adhesion showed an increase at lower temperatures, but the compliance of the PVB interlayer was reduced. Based on the interlayer thickness range tested, the post-crack response of laminated glass is shown to be thickness dependent.

Author
M A Samienean Et Al
Origin
Unknown
Journal Title
Int J Impact Engineering 111 January 2018 177-186 (Open Access) www.Sciencedirect.com/Science/Article/Pii/S0734743X17304608
Sector
Flat glass
Class
F 4048

Request article (free for British Glass members)

Temperature Effects On Laminated Glass At High Rate
Int J Impact Engineering 111 January 2018 177-186 (Open Access) www.Sciencedirect.com/Science/Article/Pii/S0734743X17304608
F 4048
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.