In industrially melted amber glass the logarithm [Fe2+]/[Fe3+] shows no linear dependence on the logarithm of oxygen partial pressure. This nonlinearity is due to the interaction between iron and sulfur which can be described by means of a simple oxygen balance model. The change of chemically dissolved oxygen as a function of the oxygen partial pressure depends on the redox state and has a minimum at intermediate oxygen partial pressures. In this region small variations of reducing additions in the batch cause large variations of oxygen partial pressure.

Author
H Muller-Simon
Origin
Huttentechnische Vereinigung Deutschen Glasindustrie, (Hvg) Germany
Journal Title
Glastech Ber Glass Sci Technol 70 12 1997 389-391
Sector
General
Class
G 1757

Request article (free for British Glass members)

Temperature Dependence Of The Redox State Of Iron And Sulfur In Amber Glass Melts
Glastech Ber Glass Sci Technol 70 12 1997 389-391
G 1757
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.