Temperature Control Of Poiseuille Flow With Particular Application To Flow Of Molten Glass.

The problem is that of controlling the temperature distribution of a fluid in fully developed laminar flow through a circular tube. It is assumed that suitable heating and cooling are available in a refractory casing surrounding the tube and that in its passage through a section of the tube and that in its passage though a section of the tube given length the mean temperature of the fluid has to be reduced (or increased) by a specified amount.

Author
D.E. Bourne Et Al
Origin
Unknown
Journal Title
Int.J.Heat Mass Transfer, 1976, 19 (9) 1045-55
Sector
Primary Papers
Class
PP 601

Request article (free for British Glass members)

Temperature Control Of Poiseuille Flow With Particular Application To Flow Of Molten Glass.
Int.J.Heat Mass Transfer, 1976, 19 (9) 1045-55
PP 601
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 10 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.