From Technology To The Science Of Glass/Metal And Ceramic/Metal Sealing

Current understanding of the conditions under which two materials can be joined to form strong and vacuum-tight seals is reviewed.

Author
J A Pask
Origin
University Of California, Berkeley
Journal Title
Ceramic Bulletin 1987 66 11 1587-1592