Technology Change Repositions Glass Block

The recent renewed popularity of glass block in the United States is attributed partly to the replacement of the traditional mortar for installation by silicone.

Author
M S Takish
Origin
Dow Corning Corp
Journal Title
Glass Digest December 15 1990 61-62