Technological Properties Of Glasses For Medical Purposes

Results of viscosity measurements on various Soviet glasses for pharmaceuticals containers are presented and workability characteristics are discussed.

Author
G S Galakhova, A S Kutukov, T I Povolotskaya
Origin
All Union Institute Of Medical Polymers
Journal Title
Glass And Ceramics 1988 45 1-2 18-20