Technological Peculiarities Of Electric Melting Of Houshold Glass

The need for careful selection of batch materials and temperature control throughout the melting process is discussed with particular reference to trials on an electric furnace with molybdenum electrodes melting selenium ruby glass.

Author
V A Fedorova, A T Dymov And R I Sumenkova
Origin
Unknown
Journal Title
Glass And Ceramics Ussr 1990 47 11-12 418-419