Technological Parameters Of Briquetting Batch For Foam Glass Production

A method for preliminary briquetting foam glass batch has been developed which not only can simplify the production process, but also modify the foam glass parameters by controlling the parameters of briquette production. The parameters for preparing briquettes for foam glass based on various technological binders and the optimum binder contents are identified. It is established that denser briquettes yield foam glass of lower density.

Author
M S Garkavi & N S Kulaeva
Origin
Unknown
Journal Title
Glass & Ceramics 62 11-12 2005 379-380
Sector
Special Glass
Class
S 3187

Request article (free for British Glass members)

Technological Parameters Of Briquetting Batch For Foam Glass Production
Glass & Ceramics 62 11-12 2005 379-380
S 3187