Tailoring The Thermal Expansion Of Glass-Ceramics By Controlled Twofold Crystallisation Of Li2Di2O5 And Csalsi5012

The mechanical and optical properties of Li2Si2O5 glass-ceramics can be precisely controlled via the crystal morphology and content. However, the materials' coefficient of thermal expansion (CTE) depends on the fraction as well as the CTE of Li2Si2O5 and the residue glass phase, and therefore covers a rather narrow range between 10.2 and 11.3 *10-6 K-1 (100-400 deg C). This study presents a way to tailor the CTE of lithium disilicate-based glass-ceramics by controlled two-fold precipitation of Li2Si2O5 and CsAlSi5O12 as a minor crystal phase with high CTE from homogeneous Cs2O comprising bulk base glasses. The Cs2O content in the base glass significantly influences the nucleation and crystallisation process of Li2Si2O5 as well as the microstructure of the glass-ceramic materials.

Author
M Rampf Et Al
Origin
Ivoclar Vivadent Ag, Liechtenstein
Journal Title
Int J Appl Glass Sci 7 3 Sept/2016 285-294
Sector
Glass Ceramics
Class
GC 881

Request article (free for British Glass members)

Tailoring The Thermal Expansion Of Glass-Ceramics By Controlled Twofold Crystallisation Of Li2Di2O5 And Csalsi5012
Int J Appl Glass Sci 7 3 Sept/2016 285-294
GC 881
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 12 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.