Tailoring The Microwave Dielectric Properties Of Ca4Ta2Ti012 Ceramics Through Glass Addition

Microwave dielectric properties of polycrystalline Ca5Ta2TiO12 ceramics have been tailored using different glass additives. Several glasses such as B2O3, SiO2, B2O3-SiO2, ZnO-B2O3,Al2O3-SiO2, Al2O3-B2O3-SiO2, BaO-B2O3-SiO2, MgO-B2O3-SiO2, ZnO-B2O3-SiO2, PbO-B2O3-SiO2, and 2MgO-Al2O3-5SiO2 were added to calcined Ca5Ta2TiO12 powder in different weight percentages.

Author
P V Bijumon & M T Sebastian
Origin
Regional Research Laboratory, Trivandrum, India
Journal Title
J Am Ceram Soc 88 12 2005 3433-3439
Sector
Glass Ceramics
Class
GC 650

Request article (free for British Glass members)

Tailoring The Microwave Dielectric Properties Of Ca4Ta2Ti012 Ceramics Through Glass Addition
J Am Ceram Soc 88 12 2005 3433-3439
GC 650
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
10 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.