Systems Approach To Hot End Glass Handling

Some applications of Dura Temp graphite-filled silicone material as a substitute for asbestos for handling hot containers are described.

Author
G A Jakes
Origin
Productivity Plus
Journal Title
Glass International 1987 December 29-30