System For The Collection And Processing Of Data Be Electron Microprobes For The Microvolumetric Analysis Of Glass

The use of a specially developed system for recording and processing data by means of electron microprobes has facilitated the analysis of glasses which are difficult or impossible with conventional microprobe techniques.