Synthetic Turf Sand

Flexsand is a newly developed product for use as infill material in artificial grass. The product consists of special graded silica sand coated with a proprietary kind of rubber.

Author
Un-named
Origin
Unknown
Journal Title
Industrial Minerals October/05 69
Sector
General
Class
G 3053

Request article (free for British Glass members)

Synthetic Turf Sand
Industrial Minerals October/05 69
G 3053