Synthesis Of Silica Glasses Doped With Siaion Phosphors By Supercritical Drying

Silica gels and glasses doped with SiAION phosphors have been synthesized by the sol-gel method. Only after half a day of supercritical drying, the dried gels with many mesopores and high surface-specific area were obtained. The chromaticity of the gels can be controlled to vary widely from blue to yellow by changing the heating temperature, SiAION concentration, and sample thickness. The thermal dependence of photoluminescence of the glass is similar to that of SiAION powder.

Author
H Segawa Et Al
Origin
Nat Inst Mat Sci Namiki, Japan
Journal Title
Int J Appl Glass Sci 8 2017 247-252
Sector
Special Glass
Class
S 4395

Request article (free for British Glass members)

Synthesis Of Silica Glasses Doped With Siaion Phosphors By Supercritical Drying
Int J Appl Glass Sci 8 2017 247-252
S 4395
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.