Synthesis Of Glass Powder Precursors In The Bao-Al203-Si02 And Bao-Zno-Al203 Systems By The Sol-Gel Route

This paper describes the chemical synthesis of amorphous batch powders in these systems and discusses the effect of various factors on the synthesis and characteristics of the xerogels.

Author
Y-J. Du Et Al
Origin
Warwick University, Uk
Journal Title
Physics & Chem Of Glasses 33 6 1992 228-232
Sector
Special Glass
Class
S 701

Request article (free for British Glass members)

Synthesis Of Glass Powder Precursors In The Bao-Al203-Si02 And Bao-Zno-Al203 Systems By The Sol-Gel Route
Physics & Chem Of Glasses 33 6 1992 228-232
S 701