Synthesis And Properties Of Fluorophosphate Glasses

Glass compositions from the AlF3-(Ca+Sr+Ba) F2-P2O5 system were synthesised under varied melting conditions. Optical properties such as ultraviolet absorption edge, infrared transmission, temperature coefficient of refractive index, and absorption coefficients at 1.32nm were determined.