Switching Characteristic Of Barium Vanadate Glasses Doped With Iron Oxide

Semiconducting barium banadate glasses (BVG) doped with iron were prepared in order to investigate their switching characteristics. Switching in these semiconducting glasses was found to follow the electrothermal model. Structural modifications in the glassy matrix occurred and appeared after the first switching. The activation energy for switching was calculated and the value found to be lower than that estimated from dc conductivity measurements. The results show a discontinuity for the threshold voltage with Fe3+ content.

Author
I A Gohar Et Al
Origin
Mansourar University, Egypt
Journal Title
Phys Chem Glasses 38 1 1997 37-41
Sector
Special Glass
Class
S 1120

Request article (free for British Glass members)

Switching Characteristic Of Barium Vanadate Glasses Doped With Iron Oxide
Phys Chem Glasses 38 1 1997 37-41
S 1120
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.