Swabbing On The Run

All four high speed tandem IS machines at Ardagh's Moerdijk glass container plant near Rotterdam have been equipped with specially developed robots to perform essential mould swabbing duties. The Ardagh Glass project team responsible for this innovative technology has worked closely with Heye International and robotics specialist Socabalec to create a system that provides significant productivity and cost saving benefits, which are described in this article.