Surface Modificaiton Of Tellurite Glass By Thermal Poling Accompanied With Ion Implantation In A Solid-State Phase

A new technique for surface modification of glass, with which thermal poling and ion implantation in a solid state phase are simultaneously accomplished has been developed.

Author
S Ukon Et Al
Origin
Kyoto University, Japan
Journal Title
Phys Chem Glasses 49 5 2008 285-288
Sector
Special Glass
Class
S 3511