Surface Energy And Structure Effects On Surface Crystallization

The shape of a critical cluster formed at a planar surface of a solid was determined taking into account both interfacial contributions and elastic terms in the expression for free enthalpy of cluster formation. The shape of critical clusters may change continuously from a sphere in the ambient solid tangent to the interface via a hemisphere to a circular nearly planar layer depending on the values of the specific surface energies (cluster-air, ambient phase-air and ambient phase-cluster phase). The work of formation of critical clusters formed at or near planar interfaces is significantly reduced compared with cluster formation in the bulk of the matrix. This reduction is even more significant for solids with a rough surface structure.

Author
J Schmelzer Et Al
Origin
Fachberich Physik Der Univ Rostock, Germany
Journal Title
Schott Research 1993-1995 195-213
Sector
Special Glass
Class
S 1161b

Request article (free for British Glass members)

Surface Energy And Structure Effects On Surface Crystallization
Schott Research 1993-1995 195-213
S 1161b
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.