Surface Damage Resistance Of Gel-Derived Oxycarbide Glasses: Hardness, Toughness And Scratchability

Gel-derived oxycarbide glasses have atomic network structures similar to that of vitreous silica glass but with carbon-rich regions consisting of SCi4 tetrahedra and C-Si-O bonds finely dispersed in the glass. Therefore, oxycarbide glasses exhibit the so-called "anomalous" hardness behaviour, similar to silica-rich glasses, with a substantial densification-strain component beneath the indenter.

Author
T Rouxel Et Al
Origin
Universite De Rennes, France
Journal Title
J Am Ceram Soc 84 10 2001 2220-2224
Sector
Special Glass
Class
S 2270

Request article (free for British Glass members)

Surface Damage Resistance Of Gel-Derived Oxycarbide Glasses: Hardness, Toughness And Scratchability
J Am Ceram Soc 84 10 2001 2220-2224
S 2270